MILLING-ZINC

fabrication millingg

 

During the milling process used a zinc thickness of 1 millimeter. The design is reflected in the creation of 2D file which bending procedure would  assume 3d shape of a sphere, and as such is designed as a small table lamp that had four legs, central / inner part with a hole for the possible installation of lighting and eight side portions to form a spherical shape.

During this process there has been a mistake when setting the controls in RhinoCam, where small contiguous parts were cut from the outside insted  of cutting from  inside so that the main holders were torn during this process. On the other hand, it is noted that the material behaves very well during this process, particularly for large parts, leaving a very accurate curvature  and clean forms.